Hot Work Tool Steel bar 1.2367/X38CrMoV5-3 – GMTC

1.2367

  • X38CrMoV5-3

SpecificationEN ISO 4957

It has high thermal fatigue resistance. In addition, GMTC has the remelting technique that can improve its grain size, segregation, cleanliness, and purity.

Quick Navigation

Inquiry

Introduction

Product properties

˙Small dimensional variation

˙Impact resistance at high temperatures

˙Good machinability

Industrial Applications

˙Die casting mold

˙Hot forging mold

˙Extrusion mold

˙Injection mode

˙Stamping mold

˙Hot rolling

˙Hot shearing blade

Specifications

Chemical composition (wt. %)

Element
C
Si
Mn
P
S
Cr
Mo
V
Min.
0.35
0.30
0.30
-
-
4.80
2.70
0.40
Max.
0.40
0.50
0.50
0.030
0.020
5.20
3.20
0.60

Physical Property

Density (g/cm^3)
7.85

Modulus of elasticity

Temperature (℃)
Gpa
500
176
600
165

Thermal Expansion Coefficient

Temperature (℃)
10^-6/℃
500
12.9
600
13

Thermal Conductivity

Temperature (℃)
W/m·K
500
34.2
600
34.9

Mechanical Property

Items
Annealed
Hardness After Quenching (hardenability) (HRC)
50 min.
Hardness (HBW)
229 max.

Size Ranges

Products
Diameter (mm)
Length (mm)
Rolled bar
10~95
3,000~5,700
Forged bar
95.2~590
3,000~5,700
Billet
130x130, 140x140, 150x150, 160x160
7,000 max
Flat bar
80x80 (min.)
Based on the customer needs

File Download

Download

A more detailed description of the products, their characteristics, applications, and quenching as well as tempering conditions

Related Application

Click any of application links below to view their detailed introduction

The product has been added to the inquiry form!

COOKIES

The website uses the browser’s cookies to give you the best user experience. The Cookies we used include the third party cookies. For more information, see our Privacyand Cookies Policies. By continuing to browse our website or closing this prompt, you agree to accept our Terms of Use of our website.

I agree

前往舊版網站
獲得完整瀏覽體驗

您所使用的裝置版本不支援新版網站的部分功能,請移轉至舊版網站獲得完整瀏覽體驗

立即前往